FAG bearing grinding line defect causes the formation of spiral

FAG bearings in the grinding process, the surface of their work is done by high-speed rotation of the grinding wheel, grinding so if you do not follow the operating instructions for operation and adjust the device, it will work in the bearing surface of various defects, resulting in affect the overall quality of the bearing. Bearing in precision grinding, due to the rough demanding work surface grinding marks often appear to the naked eye can trace its surface grinding are the following. Performance of cross spiral traces traces happen mainly due to poor wheel bus straight, there is uneven phenomenon, in the grinding, the grinding wheel is only partial contact with the workpiece when the workpiece or the wheel back and forth several times after exercise, in performance will reproduce the cross piece and the helix can be observed visually. The pitch of the helix and the workpiece table speed, the size of workpiece speed, but also with the wheel axis is not parallel to the guide lines and the table.
(A) the main helical form:
1 Dresser bad, not chamfered corners, unused coolant to be trimmed;
2 table guide rail lubricant too much, resulting workbench floating;
3 machine precision is not good;
4 grinding pressure is too big.
(B) The specific reasons for the formation of helix:
1.V shaped rail rigidity bad, when an offset grinding wheel, but wheel edge in contact with the work surface;
2 noisy wheel dressing table commutation speed is unstable, accuracy is not high, so that the edge of a grinding wheel dressing slightly less;
3. Workpiece itself rigidity;
4 wheel has broken too flaking grit and the workpiece grinding wheel under the iron plot attached to the surface, this should be a good dressing wheel with cooling water wash or scrub clean;
5 wheel dressing well, there are local projections and so on. Surface appears scaly scaly surface reproduces the main reason is due to traces of grinding wheel cutting edge is not sharp enough, in the grinding occurs when "eating to live" phenomenon, when large vibration.


Previous: Why bearing will generate noise it?
Next: Plastic machinery in five categories TIMKEN bearing structure performance analysis

Hot Products:
Product Model Inside Diameter Outside Diameter Thickness
7230ADB NSK 150 270 45
7030ADB NSK 150 225 35
【TradeBearings News Statement】

1.The news above mentioned with detailed source are from internet.We are trying our best to assure they are accurate ,timely and safe so as to let bearing users and sellers read more related info.However, it doesn't mean we agree with any point of view referred in above contents and we are not responsible for the authenticity. If you want to publish the news,please note the source and you will be legally responsible for the news published.
2.All news edited and translated by us are specially noted the source"TradeBearings".
3.For investors,please be cautious for all news.We don't bear any damage brought by late and inaccurate news.
4.If the news we published involves copyright of yours,just let us know.